Test results
Mineral
Airgrinder have carried out tests with the following results:
| Material |
Moisture In |
Moisture Out |
Reduction |
|
Hydroxide sludge
 |
45% |
15% |
30% |
|
Blast furnace sludge
 |
40% |
5% |
35% |
|
Brown coal
 |
54% |
3% |
51% |
|
Recycled material residue - drying and separation
 |
|
|
|
Contact us for further info or if you are interested in conducting a test on your specific material.